Sign In | Join Free | My disqueenfrance.com
China Changzhou Victory Technology Co., Ltd logo
Changzhou Victory Technology Co., Ltd
Changzhou Victory Technology Co., Ltd
Verified Supplier

2 Years

Home > Precision Alloy >

Supply 1J79/1J85/1J87 Permalloy Precision Alloy Wire With Factory Price

Changzhou Victory Technology Co., Ltd
Trust Seal
Verified Supplier
Credit Check
Supplier Assessment
Contact Now

Supply 1J79/1J85/1J87 Permalloy Precision Alloy Wire With Factory Price

  • 1
  • 2

Brand Name : Victory

Model Number : Permalloy 80

Place of Origin : China

MOQ : 50

Price : $25-$40

Payment Terms : L/C, T/T, Western Union, MoneyGram

Supply Ability : 200 tons per month

Delivery Time : 5-21 days

Packaging Details : Standard Export Wooden Cases Ex.Gross Weight Under 20kg=Carton Box/Gross Weight over 20 kg=Plywood Box Or as per Request

Material : NiFe

Certificate : ISO9001

Shape : wire, strip, foil, sheet

Resistivity : 0.56

density : 8.75g/cm3

size : customized

Standard : GB/ASTM/AISI/ASME

Condition : Bright, Annealed, Soft

Application : Industrial Magnet

Curie Point : 400℃

HCR : 30

Feature : high initial permeability

Contact Now

High Permeability Soft Magnetic Alloy


Supply 1J79/1J85/1J87 Permalloy Precision Alloy Wire With Factory Price


Soft magnetic materials are essential components in both the power and electronics industries. In the power industry, these materials are used in high magnetic fields to achieve a high magnetic induction and low core loss. On the other hand, in the electronics industry, soft magnetic materials are mainly used in low or medium magnetic fields, with a high magnetic permeability and low coercive force.

When it comes to high frequencies, thin strips or alloys with higher resistivity are preferred. This is because, in soft magnetic materials, alternating magnetic eddy currents are induced inside the material, resulting in loss. The higher the frequency of the alternating magnetic field, the greater the eddy current losses, and the more the magnetic field is reduced. Therefore, to minimize these losses, the material must be made thinner, usually in the form of a sheet or tape. Additionally, the surface of the material is coated with an insulating layer or an oxide insulating layer is formed on the surface using certain methods. One common method is to use magnesium oxide electrophoresis coating.

In summary, soft magnetic materials are crucial in both the power and electronics industries. Their properties are carefully chosen depending on the application and frequency range. To minimize losses due to eddy currents, the material is made thinner and coated with an insulating layer.

Applications

High sensitivity and small power transformers, magnetic amplifiers, relays, chokes, magnetic heads for magnetic recording devices, magnetic shields, various tape wound cores, cut cores, and laminated cores used in weak magnetic fields.

Material C P S Mn Si Ni Cr Co Mo Cu Fe
Max
Permalloy80 0.03 0.020 0.020 0.3-0.6 0.15-0.30 79.0-81.0 - - 4.8-5.2 ≤0.2. Rest

rial Shape Class Thickness or Diameter mm Magnetic permeability in 0.08A/m magnetic field intensity μ0.4(mH/m) Maximum permeability μm(mH/m) Coercivity(under saturation magnetic induction)Hc/A·m-1 Saturation magnetic induction Bs/T
not less than no greater than
Permalloy80 Cold rolled strip 0.03-0.04 18000(22.5) 80000(100) 3.6 0.70
0.05-0.09 28000(35) 110000(137.5) 2.4 0.70
0.10-0.19 30000(37.5) 150000(187.5) 1.6 0.70
0.20-0.34 40000(50) 180000(225) 1.2 0.70
0.35-1.00 50000(62.5) 250000(312.5) 0.8 0.70
1.10-2.50 40000(50) 150000(187.5) 1.2 0.70
0.03-0.04 30000(37.5) 110000(137.5) 2.4 0.70
0.05-0.09 40000(50) 140000(175) 1.6 0.70
0.10-0.19 50000(62.5) 180000(225) 1.2 0.70
0.20-0.34 60000(75) 200000(250) 1.0 0.70
0.35 55040(68.8) 260000(325) 0.7 0.70
Hot rolled tape 4.5-20 30000(37.5) 100000(125) 1.6 0.70
Hot forged bar 20-100 30000(37.5) 100000(125) 1.6 0.70

Material Shape Class Thickness or Diameter mm Magnetic permeability in 0.08A/m magnetic field intensity μ0.4(mH/m) Maximum permeability μm(mH/m) Coercivity(under saturation magnetic induction)Hc/A·m-1 Saturation magnetic induction Bs/T
not less than no greater than
Permalloy80 Cold rolled strip 0.03-0.04 18000(22.5) 80000(100) 3.6 0.70
0.05-0.09 28000(35) 110000(137.5) 2.4 0.70
0.10-0.19 30000(37.5) 150000(187.5) 1.6 0.70
0.20-0.34 40000(50) 180000(225) 1.2 0.70
0.35-1.00 50000(62.5) 250000(312.5) 0.8 0.70
1.10-2.50 40000(50) 150000(187.5) 1.2 0.70
0.03-0.04 30000(37.5) 110000(137.5) 2.4 0.70
0.05-0.09 40000(50) 140000(175) 1.6 0.70
0.10-0.19 50000(62.5) 180000(225) 1.2 0.70
0.20-0.34 60000(75) 200000(250) 1.0 0.70
0.35 55040(68.8) 260000(325) 0.7 0.70
Hot rolled tape 4.5-20 30000(37.5) 100000(125) 1.6 0.70
Hot forged bar 20-100 30000(37.5) 100000(125) 1.6 0.70

Supply 1J79/1J85/1J87 Permalloy Precision Alloy Wire With Factory Price


Product Tags:

Precision Alloy Bright

      

Precision Alloy Annealed

      

High Permeability soft iron alloy

      
China Supply 1J79/1J85/1J87 Permalloy Precision Alloy Wire With Factory Price wholesale

Supply 1J79/1J85/1J87 Permalloy Precision Alloy Wire With Factory Price Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: Changzhou Victory Technology Co., Ltd
*Subject:
*Message:
Characters Remaining: (0/3000)
 
Inquiry Cart 0